Table 4 Z\(g), Z\(gb), RB, Ceff and αe of the Cd0.40Mn0.60ZnO2 annealed nanocomposite samples.

From: Comprehensive study of optical, photocatalytic and dielectric properties of Cd0.40Mn0.60ZnO2 annealed nanocomposites

Tann

(oC)

Z\(g)

(MΩ)

Z\(gb)

(MΩ)

RB

(MΩ)

Ceff

(nF)

αe x10− 24

(cm3)

200

2.93

9.31

11.10

9

9.96

300

2.20

6.35

10

10

5.76

400

3.19

9.51

11.10

7.94

9.83

500

3.25

10.70

14.30

7.48

9.42

600

2.25

7.65

10

10

9.08