Fig. 4: Coaxial nanofibers fabricated using electrospinning method. | Communications Materials

Fig. 4: Coaxial nanofibers fabricated using electrospinning method.

From: Crafting high-temperature stable and hydrophobic nanofiber membranes for particulate matter filtration

Fig. 4

a Nanofiber fabrication process and scanning electron microscopy (SEM) images of ampicillin-loaded polycaprolactone (PCL) nanofibers with various flow rates and concentrations (wt%). The fabricated nanofibers are denoted as CR (core nanofiber), CS1 (core-shell nanofiber 1), and CS2 (core-shell nanofiber 2). The diameter of the fabricated nanofibers is in the range of 400–700 nm. (reproduced with permission from,167 copyright (Elsevier B.V., 2016)). b The nanofiber fabrication process and SEM images of coaxial nanofibers comprising polyacrylamide (PAAm) as a core and L-Arginine (L-Arg)-combined keratin (AloKr) as a shell. (reproduced with permission from,168 copyright (Elsevier B.V., 2024)).