Fig. 3: Changes in crystal structure with the increased number of chemical elements and changes after the stability test.

XRD patterns of NiOx, NiFe0.3Ox, and NiFe0.3MoOx sprayed on glass substrates. XRD of NiFe0.3MoOx as-produced and after stability test (1000 CVs + 24 h CA) was sprayed on FTO substrates.