Abstract
For the thermal degradation of polyisobutylene, the effects of physical factors such as pressure in the reaction vessel and volume and molecular weight of the molten polymer matrix constituting the reaction media on the formation of the volatile oligomers were examined by a kinetic approach with measurements of composition ratios for terminal monoolefins [(TTD)p, (TVD)p, (TTD)t, and (TVD)t)]. The observed values of the composition ratios [TTD]p/[TVD]p and [TTD]t/[TVD]t are kept constant independently of changes in the physical factors. On the other hand, the ratios [TTD]p/[TTD]t and [TVD]p/[TVD]t do not depend on pressure and initial mass of sample, but depend on the initial molecular weight of sample. These values decrease clearly as the initial molecular weight decreases. It could be deduced that the decrease in molecular weight of the matrix decreases concentration ratio of two types of terminal macroradicals ([Rp·]/[Rt·]). According to the proposed kinetics of a chain mechanism including diffusion-controlled termination, a marked decrement of the radical concentration ratio suggests that the rate of termination increases with decrease in molecular weight of the matrix and that resulting decrement of kinetic chain length depresses the formation of the primary terminal macroradical (Rp·) in the depropagation step.
Similar content being viewed by others
Log in or create a free account to read this content
Gain free access to this article, as well as selected content from this journal and more on nature.com
or
References
I. Mita and K. Horie, “Degradation and Stabilization of Polymers-1,” H. H. G. Jellinek, Ed., Elsevier, New York, N.Y., 1983, p 235.
I. Mita “Aspects of Degradation and Stabillzation of Polymers,” H. H. G. Jellinek, Ed., Elsevir, New York, N.Y., 1978, p 247.
T. Sawaguchi, T. Takesue, T. Ikemura, and M. Seno, Macromol. Chem. Phys., 196, 4139 (1995).
T. Sawaguchi, T. Ikemura, and M. Seno, Macromol. Chem. Phys., 197, 215 (1996).
Y. Tsuchiya and K. Sumi, J. Polym. Sci., A-1, 7, 813 (1969).
T. Kuroki, T, Sawaguchi, K. Suzuki, S. Ide, and T. Ikemura, Polymer, 24, 428 (1983).
Y. Sakaguchi and I. Sakurada, Kobunshi Kagaku, 5, 242 (1948).
V. Srinivasan and S. V. Babu, Polym. J., 17, 525 (1985).
G. G. Cameron and G. P. Kerr, Eur. Polym. J., 4, 709 (1968).
G. G. Cameron, Makromol. Chem., 100, 255 (1967).
G. G. Cameron J. M. Meyer, and I. T. McWalter, Macromolecules, 11, 696 (1978).
T. G. Fox and P. J. Flory, J. Phys. Colloid Chem., 55, 221 (1951).
M. Smoluchowski, Z. Phys. Chem., 92, 129 (1918).
P. G. de Gennes,“Scaling Concepts in Polymer Physics,” Cornell University Press, New York, N.Y., 1979.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Sawaguchi, T., Seno, M. Effects of Molecular Weight of Reaction Media on Formation of Volatile Oligomers by Thermal Degradation of Polyisobutylene. Polym J 28, 392–399 (1996). https://doi.org/10.1295/polymj.28.392
Issue date:
DOI: https://doi.org/10.1295/polymj.28.392