Table 1 The MWC and BD of waterlogged archaeological wood and reference wood samples

From: Degradation condition and microbial analysis of waterlogged archaeological wood from the second shipwreck site on the northwestern continental slope of the South China Sea

Samples

Maximum moisture content (%)

Basic density (g/cm3)

S1

22.95 (±1.26)

1.22 (±0.03)

S2

28.69 (±2.39)

1.10 (±0.03)

S3

144.38 (±5.07)

0.43 (±0.02)

R1

19.44 (±1.56)

1.23 (±0.02)

R2

114.19 (±2.77)

0.52 (±0.02)