Table 1 Electrical parameters for simulation.
From: Experimental proof of Joule heating-induced switched-back regions in OLEDs
Model | Parameter | Value | |
|---|---|---|---|
Recombination | j00 | 40 A/cm² | |
Ea,0 | 2.74 eV | ||
nid | 1.55 | ||
p-system | Linear | Non-linear | |
α | 1.0 | 4.1 | |
jref | 0.6 mA/cm² | 8.1 mA/cm² | |
Ea,0 | 0.275 eV | 0.25 eV | |
n-system | Linear | Non-linear | |
α | 1.0 | 3.07 | |
jref | 0.05 mA/cm² | 3.3 mA/cm² | |
Ea,0 | 0.5 eV | 0.325 eV |