Table 1 Relative third-order susceptibility of tBLG compared with the THG intensity of neutral MLG at various sample positions at Vg = 0 V (nongated) and –1.8 V
From: Enhanced third-harmonic generation by manipulating the twist angle of bilayer graphene
Sample position \({\raise0.5ex\hbox{$\scriptstyle {\chi _{tBLG}^{(3)}}$}\kern-0.1em/\kern-0.15em \lower0.25ex\hbox{$\scriptstyle {\chi _{MLG}^{(3)}}$}}\) | 1 (MLG) | 2 | 3 | 4 | 5 | 6 | 7 |
|---|---|---|---|---|---|---|---|
Vg = 0 V | 1.0 | 1.03 | 0.94 | 0.91 | 1.30 | 1.46 | 0.91 |
Vg = –1.8 V | 3.67 | 2.54 | 2.46 | 2.71 | 3.86 | 3.02 | 2.72 |