Table 4 Degree of conversion and standard deviation for each resin cement with self-cure and dual-cure protocols.
Polymerization mode | Resin cements | DC in% (±SD) |
|---|---|---|
Dual-cure | R-U | 73.3 (±0.0)B |
GC-O | 75.2 (±0.0)B | |
TTC | 70.2 (±0.0)C | |
N-U | 78.4 (±0.0)A | |
PSA-U | 73.6 (±0.0)B | |
SCP | 73.1 (±0.0)B | |
MHA | 74.2 (±0.1)B | |
Self-Cure | R-U | 68.4 (±0,0)C |
GC-O | 64.3 (±0.1)D | |
TTC | 60.3 (±0.1)E | |
N-U | 69.1 (±0.1)C | |
PSA-U | 62.3 (±0.0)E | |
SCP | 68.4 (±0.0)C | |
MHA | 65.8 (±0.1)D |