Fig. 2: Characterization of PePMMAs.

a, b SAXS data of monolith with (a) 40 wt% and (b) 30 wt% PMMA loading including d (nm). DSC thermograms with (c) 40 wt% and (d) 30 wt% PMMA loading including Tgs. The data was recorded during the second heating cycle (10 °C min-1, N2) e Stress-strain curves at RT. f Impact resistance of impact-modified PMMA (orange) and PePMMA(40, 2.5) (gray).