Table 5 Wetting parameters for 20 µL sessile water drops on PP and PTFE

From: The measurement of the surface energy of solids using a laboratory drop tower

Parameter

PP

PTFE

γ S

mJ/m2

31.0481

20.9384

γ SL

mJ/m2

70.2298

64.9132

κ

0.54818

0.64825

\(\Omega _S^{\kappa {\prime}}\)

mm2

11.3585

13.1434

\(\Omega _S^G\)

mm2

10.3006

12.7835

\(\Omega _L^{\kappa {\prime}}\)

mm2

28.2898

28.4698

\(\Omega _L^G\)

mm2

28.3079

28.4293

\(\Omega _{SL}^{\kappa {\prime}}\)

mm2

13.6414

11.8566

\(\Omega _{SL}^G\)

mm2

14.6993

12.2164

γ L \(\Omega _L^\kappa\)

µJ

2.0595

2.0726

γ L \(\Omega _L^G\)

µJ

2.0608

2.0690

γ S \(\Omega _S^\kappa\)

µJ

0.3527

0.2752

γ S \(\Omega _S^G\)

µJ

0.3198

0.2677

γ SL \(\Omega _{SL}^{\kappa {\prime}}\)

µJ

0.9580

0.7696

γ SL \(\Omega _{SL}^G\)

µJ

1.0323

0.7930

z c κ

mm

0.8146

0.8885

z cG

mm

0.7596

0.8552

µJ

3.3702

3.1174

A G

µJ

3.4130

3.1303

W M =A G A κ

µJ

0.0428

0.0129

θκ

°

92.04

99.62

θ G

°

90.86

100.99