Fig. 2: The pre-factor for the nucleation rate as a function of the maximum shear rate at the maximum undercooling temperature of liquid Vit 106 (Zr57Cu15.4Ni12.6Al10Nb5), processed in vacuum using the ISS-EML.

The dashed line is included as a guide to the eye. (Adapted from Fig. 2 in ref. 27).