Table 3 POMaC pre-polymer spin coating settings and resulting film thickness.

From: Biodegradable elastomeric circuit boards from citric acid-based polyesters

Spread Stage

Spin Stage

Thickness (μm)

RPM

Acc.

Time (s)

RPM

Acc.

Time (s)

750

172

15

850

172

10

412 ± 13

  1. Thickness reported as mean ± standard error of the mean.
  2. RPM revolutions per minute, Acc. acceleration, s seconds.