Table 2 Data extraction of 2Pr and 2Ec for thin films in Fig. 2d

From: The enhanced ferroelectric properties of flexible Hf0.85Ce0.15O2 thin films based on in situ stress regulation

Bent & annealed (mm)

Unbent

−12.5

−10

−7.5

2Pr (μC/cm2)

9.7

15.2

16.6

9.5

2Pr increase percentage

56.7

71.1

−2.1