Fig. 11 | npj Materials Degradation

Fig. 11

From: Time-dependent in situ measurement of atmospheric corrosion rates of duplex stainless steel wires

Fig. 11

Corrosion morphology of 2205–3 DSS (1.2 YS) wire after 524 days exposure: a a localised corrosion site with bc showing transgranular SCC, d an elongated localised corrosion site with ef showing the selective dissolution of either the ferrite or austenite within these sites. Narrow SCC cracks were observed at the bottom of those sites, gh indicating corrosion by selective attack, i showing a corrosion pit with no sign of selective corrosion. ae, gi BSE-SEM images and f SE-SEM image

Back to article page