Fig. 2
From: Time-dependent in situ measurement of atmospheric corrosion rates of duplex stainless steel wires

3D visualisations of the reconstructed volume of lean 2202–1 (YS) DSS showing a, b the corrosion morphology after 83 days of exposure, c, d after 177 exposure days, and e after 542 days. In b and d the material lost by corrosion has been segmented (red)