Table 1 Limited degradation of surface area-to-volume ratio after annealing in oxidative environment.
Volume fraction NPG | Surface area NPG/NPG volume (nm−1) | |
|---|---|---|
NPG-AuAgPt3 (annealed in air) | 0.501 | 0.479 |
NPG-AuAgPt3 | 0.520 | 0.576 |
Volume fraction NPG | Surface area NPG/NPG volume (nm−1) | |
|---|---|---|
NPG-AuAgPt3 (annealed in air) | 0.501 | 0.479 |
NPG-AuAgPt3 | 0.520 | 0.576 |