Fig. 12: Differences in critical [F−] between this work and the literature.
From: Degradation of thermal oxide film on pure titanium in an acidic environment containing fluoride
![Fig. 12: Differences in critical [F−] between this work and the literature.](http://media.springernature.com/full/springer-static/image/art%3A10.1038%2Fs41529-022-00275-9/MediaObjects/41529_2022_275_Fig12_HTML.png)
Summary of the critical [F−] in the literature.
From: Degradation of thermal oxide film on pure titanium in an acidic environment containing fluoride
![Fig. 12: Differences in critical [F−] between this work and the literature.](http://media.springernature.com/full/springer-static/image/art%3A10.1038%2Fs41529-022-00275-9/MediaObjects/41529_2022_275_Fig12_HTML.png)
Summary of the critical [F−] in the literature.