Table 2 EIS fitting results of HNSS1 and HNSS2.
From: Effect of nitrogen content on corrosion behavior of high-nitrogen austenitic stainless steel
Rs / Ω cm2 | Q / Ω−1 sn cm−2 | n | Rf / Ω cm2 | dox / nm | |
|---|---|---|---|---|---|
HNSS1 | 10.36 ± 0.05 | (5.34 ± 0.15) × 10−5 | 0.90 | (1.50 ± 0.10) × 105 | 12.7 |
HNSS2 | 12.21 ± 0.05 | (5.55 ± 0.10) × 10−5 | 0.87 | (1.73 ± 0.08) × 105 | 13.5 |