Table 1 EDS analysis of the LPBF sample and wrought sample.

From: Oxidation kinetic behavior and microstructure mechanism of GH3536 alloy fabricated by laser powder bed fusion

  

O

Cr

Fe

Ni

Mn

wt.%

At.%

wt.%

At.%

wt.%

At.%

wt.%

At.%

wt.%

At.%

LPBF

a

31.58

60.16

61.13

35.82

\

\

0.71

0.36

6.56

3.64

b

32.55

61.09

66.54

38.42

0.54

0.29

0.35

0.18

\

\

c

1.94

6.54

19.63

20.36

19.91

19.22

56.63

52.02

1.87

1.83

Wrought

a

32.99

62.03

44.99

26.02

0.86

0.46

2.91

1.49

18.22

9.97

b

39.46

67.97

59.28

31.41

0.94

0.46

0.30

0.14

\

\

c

2.68

9.37

17.73

19.05

20.55

20.55

45.12

42.93

\

\