Table 2 Electrochemical parameter of EIS.
From: Attain insensitivity to chlorine ions in magnesium alloys by impeding the diffusion process
Alloy | Solution | Rs (Ω cm2) | Rct (Ω cm2) | CPEdl | Rf (Ω cm2) | CPEf | RL (Ω cm2) | L (H cm 2) | ||
|---|---|---|---|---|---|---|---|---|---|---|
(Ω−1sn cm−2) | ndl | (Ω−1sn cm−2) | nf | |||||||
Mg | 3.5 | 13.51 | 834.9 | 0.001213 | 0.79846 | 947.1 | 1.50E-05 | 0.92503 | / | / |
10 | 10.2 | 101.8 | 0.000106 | 0.78537 | / | / | / | 40.43 | 511.1 | |
Mg-Nd-Zr | 3.5 | 14.51 | 2011 | 0.000989 | 0.71271 | 2347 | 1.30E-05 | 0.92815 | / | / |
10 | 12.26 | 1425 | 0.001179 | 0.7072 | 2236 | 1.83E-05 | 0.90577 | / | / | |