Fig. 6: FTIR colormaps of non-irradiated ZNBS samples evolved with different leaching time. | npj Materials Degradation

Fig. 6: FTIR colormaps of non-irradiated ZNBS samples evolved with different leaching time.

From: Influence of radiation on borosilicate glass leaching behaviors

Fig. 6

ac are the corresponding FTIR colormap for ZNBS1, ZNBS2 and ZNSB3 evolved with leaching time, respectively. Three peaks labeled as Roman numerals I, II, and III, correspond to the B-O-B structure at approximately 700 cm−1, the O-Si-O structure at around 780 cm−1, and the Si-related Q structure at approximately 1050 cm−1, respectively.