Table 3 EIS fitting results for the different AM Zn alloy scaffolds

From: The effect of topological design on the degradation behavior of additively manufactured porous zinc alloy

Cell unit

Rs (Ω cm2)

Cf (sn Ω1 cm2)

Rf (Ω cm2)

Qct (sn Ω1cm2)

Rct (Ω cm2)

W (Ω cm2)

Chi squared

D

10

2.53 × 108

5.36

0.051

33.9

0.037

6.05 × 105

F

4.02

2.92 × 107

2.36

0.14

32.8

0.028

5.40 × 104

G

6.66

2.71 × 107

2.96

0.13

38.7

0.011

1.24 × 104

P

3.2

1.51 × 107

3.75

0.08

97

0.03

1.93 × 104