Table 6 Volume change of the D and P scaffolds before and after 14-days immersion according Micro-CT analysis

From: The effect of topological design on the degradation behavior of additively manufactured porous zinc alloy

Specimen

D (mm3)

P (mm3)

As-polished

148

155

As-polished-center

82

85

SBF-14

132

146

SBF-14-center

73

79