Fig. 3: Examples of fracture surfaces in Mode I and II on 0WESE specimens.
From: Fracture analysis under modes I and II of adhesive joints on CFRP in saline environment

a topographic view with north detector; b topographic view with east detector; c topographic view with south detector; d topographic view with west detector; e SEM view.