Fig. 6
From: Fracture analysis under modes I and II of adhesive joints on CFRP in saline environment

Mode I and Mode II fracture surfaces, 1WESE at various magnifications (50×, 300×, 1000×, and 3000×).
From: Fracture analysis under modes I and II of adhesive joints on CFRP in saline environment