Table 4 The εL values of Ti-6Al-4V samples with different orientations in the as-fabricated and hot isostatic pressed (HIP) condition prepared by EB-PBF in ASS at 37 °C

From: The significant impact of hot isostatic pressing on the corrosion behavior of Ti-6Al-4V alloy prepared by electron beam powder bed fusion

Samples

A0

A90

B0

B90

εL (107/ V·m−1)

6.93

4.78

2.68

1.81