Extended Data Fig. 6: The multicycle tensile fracture test result of a ntDC NB with a width of ~ 200 nm. | Nature Materials

Extended Data Fig. 6: The multicycle tensile fracture test result of a ntDC NB with a width of ~ 200 nm.

From: Self-healing of fractured diamond

Extended Data Fig. 6: The multicycle tensile fracture test result of a ntDC NB with a width of ~ 200 nm.The alternative text for this image may have been generated using AI.

a, Load versus displacement curves with different healing duration timing immediately after previous fracture. b, Healing efficiency corresponding to the healing cycle in a.