Fig. 3: Ion/electron transport in SE-free Si anodes.
From: Chemo-mechanical failure mechanisms of the silicon anode in solid-state batteries

a, Lithiation curves of the SE-free Si and Si/LPSCl anodes at 0.1C. b, Lithium chemical diffusion coefficient of the LixSi alloys for different SoCs. c, Simulated crystal and amorphous LiSi3 structures before and after the melt-and-quench process. d, Simulated ionic conductivity and the corresponding activation energy of amorphous LixSi alloys for different SoCs at 300 K. e, Simulated electronic conductivity and the corresponding electron concentration of amorphous LixSi alloys for different SoCs at 300 K. f, Resistance changes in the Si anode during the lithiation process.