Extended Data Fig. 10: Characterization of catalytic stabilities.
From: Mastering the surface strain of platinum catalysts for efficient electrocatalysis

a–d, MOR CV evolutions (a), MOR mass activity evolutions (b), HER LSV evolutions (c), and HER mass activity evolutions (d) for Pt/C, PtT-2.8 and PtT-2.8-6 nm. The accelerated durability tests show 6% activity loss for PtT-2.8 toward MOR after 20,000 potential cycles and 12% activity loss for PtT-4.7 toward HER after 10,000 potential cycles, both surpassing Pt/C. e, Atomic ratio of Pt:Pd before and after the durability tests for PtT-2.8 and PtT-4.7, showing negligible compositional changes. f, g, TEM images, HAADF-STEM images, and lattice profiles of PtT-2.8 (f) and PtT-4.7 (g) after the durability tests, showing negligible structural changes.