Extended Data Fig. 4: A typical gas chromatograph of the PP pyrolysis products by STH (0.11 s power on at about 22 V and 0.99 s power off).
From: Depolymerization of plastics by means of electrified spatiotemporal heating

Inset, the gas bag used to collect the reaction products in the gas phase, which is connected downstream in the STH system.