Fig. 4: Cyclic oxidation results at 1,093 and 1,200 °C.
From: A 3D printable alloy designed for extreme environments

a,b, Cyclic oxidation results for GRX-810 and superalloy 718 at 1,093 °C (a) and 1,200 °C (b) for up to 35 h. c, Optical images of oxidation samples after 100 h at 1,093 °C and 3 h at 1,200 °C, at which the superalloy 718 sample presented catastrophic oxidation. The three samples above are all GRX-810. d, GRX-810 samples after thermal cycling for 100 h at 1,093 and 1,200 °C. Error bars represent 1 s.d.