Extended Data Fig. 8: Atomic and electronic band structures of the Se-alloyed Te-TeOx.
From: Selenium-alloyed tellurium oxide for amorphous p-channel transistors

a. Atomic structure of amorphous Se-alloyed Te-TeOx generated in DFT (Te:O atomic ratio = 1:1.2; Te:Se atomic ratio = 3:1, film density = 5.6 g/cm3). b. Projected DOS of the O 2p (red), Te 5p (dark yellow), and Se 4p (green) states in DFT-PBE.