Extended Data Fig. 5: Electrical resistivity and Hall resistivity data for a bulk single crystal of Gd3(Ru0.95Rh0.05)4Al12.

a-c, Longitudinal resistivity ρxx, Hall resistivity ρyx, and Hall conductivity σxy at various temperatures. In support of Fig. 4 of the Main Text, here we show raw data of each quantity. Direction of magnetic field ramping is indicated by black arrows, with solid lines for ∂B/∂t < 0 and dashed lines for increasing magnetic field. The magnetic field is applied along the c-axis of the crystal. The offset between curves is set to be 2 μΩcm, 2 μΩcm, and 500 Ω−1cm−1 in panels a, b, and c, respectively.