Table 3 The absorbed energy as a function of the test temperature of the WL10 and the φ1.5 mm ZrO2 ball SMATed WL10.

From: Nanostructured laminar tungsten alloy with improved ductility by surface mechanical attrition treatment

Test temperature & Samples

WL10 (Absorbed Energy, J)

φ1.5 mm ZrO2 ball SMATed WL10 (Absorbed Energy, J)

400 °C

0.375

0.875

425 °C

1

450 °C

0.375

1.75

500 °C

0.375

3.25

600 °C

0.375

5.25

700 °C

4.25

8.75