Figure 2

Strain-rate dependence of temperature-time profiles for narrow- stress-hysteresis Ni45Mn50−xInxCo5 samples at room temperature: (a) x = 13.6, T test = 293 K, and (b) x = 14.0, T test = 287 K.

Strain-rate dependence of temperature-time profiles for narrow- stress-hysteresis Ni45Mn50−xInxCo5 samples at room temperature: (a) x = 13.6, T test = 293 K, and (b) x = 14.0, T test = 287 K.