Table 1 Phase transition temperatures (M s, M f, A s, A f) from ther MT measurements, the interval between the Curie and MT temperatures (T c − M s), and the testing temperature T t for the isothermal stress–strain behaviours in Ni45Mn50−xInxCo5 samples (x = 13.6, 13.8, 14.0).

From: Elastocaloric effect and superelastic stability in Ni–Mn–In–Co polycrystalline Heusler alloys: hysteresis and strain-rate effects

Composition (at. %)

M s (K)

M f (K)

A s (K)

A f (K)

T c − M s (K)

T t (K)

x = 13.6

247.8

241.4

261.4

268.4

147

293

x = 13.8

222.9

195.4

217.4

235.5

172

293

x = 14.0

287