Figure 9
From: A Sensory Material Approach for Reducing Variability in Additively Manufactured Metal Parts

TEM image of the AM fabricated NiTi sample using laser scan distance of 35 μm showing small <5 nm precipitates along with two larger Ti2Ni precipitates.