Table 1 Machining conditions25, 26.
From: Investigation of material removal in inner-jet electrochemical grinding of GH4169 alloy
Electrolyte | NaNO3 aqueous solution |
|---|---|
Concentration | 10 wt% |
Spindle speed | 1000 rev min−1 |
Diamond grain size | 90, 120, 150, 180# |
Applied voltage | 10, 15, 20, 25 V |
Electrolyte temperature | 20, 35, 30, 35 °C |
Electrolyte pressure | 0.2, 0.3, 0.4, 0.5 MPa |
Machined depth | 3 mm |