Figure 9
From: Preparation of CH3NH3PbI3 thin films with tens of micrometer scale at high temperature

Three-dimensional AFM images of (a) PbI2 thin film fabricated by PLD and (b) prepared MAPbI3 thin film at 180 °C for 25 minutes.