Figure 6
From: Ohmic contact between iridium film and hydrogen-terminated single crystal diamond

(a) Ir and C proportion with Ar etching; (b) XPS spectra of 15 nm Ir and 3 nm Ir with Ar etching 10 sec each time of sample D.
From: Ohmic contact between iridium film and hydrogen-terminated single crystal diamond

(a) Ir and C proportion with Ar etching; (b) XPS spectra of 15 nm Ir and 3 nm Ir with Ar etching 10 sec each time of sample D.