From: Recyclable Polydimethylsiloxane Network Crosslinked by Dynamic Transesterification Reaction

Figure 2The alternative text for this image may have been generated using AI.

Solvent resistance of the crosslinked PDMS network. (a) Comparison of m swollen/m initial of crosslinked PDMS network at different swelling temperatures and periods in diphenyl ether. (b) Digital photograph exhibiting the solubility using diphenyl ether (left) and diphenyl ether/1-nonanol (right) as the solvent at 180 °C.