Figure 2
From: Non-noble, efficient catalyst of unsupported α-Cr2O3 nanoparticles for low temperature CO Oxidation

X-ray powder diffractograms for the as-obtained Cr2O3 and its calcination products (400°–800 °C). *-labelled peaks are due to the Pt/Rh sample holder.