Table 1 Fitting parameters obtained from Eq. (1) with different irradiation power density. The subscript b and d refer to bleaching and darkening, respectively.

From: Observation of photobleaching in Ge-deficient Ge16.8Se83.2 chalcogenide thin film with prolonged irradiation

Power density (W/cm2)

\({{\boldsymbol{\tau }}}_{{\boldsymbol{d}}}\)

\({{\boldsymbol{\beta }}}_{{\boldsymbol{d}}}\)

\({\boldsymbol{\Delta }}{{\boldsymbol{T}}}_{{\boldsymbol{S}}{\boldsymbol{d}}}\)

\({{\boldsymbol{\tau }}}_{{\boldsymbol{b}}}\)

\({{\boldsymbol{\beta }}}_{{\boldsymbol{b}}}\)

\({\boldsymbol{\Delta }}{{\boldsymbol{T}}}_{{\boldsymbol{S}}{\boldsymbol{b}}}\)

0.02

1200

0.97

0.9545

11000

0.93

0.053

0.05

600

0.95

0.942

10000

0.9

0.085

0.1

280

0.9

0.925

8000

0.85

0.115

0.2

150

0.85

0.907

4800

0.7

0.138

0.5

60

0.7

0.815

950

0.5

0.26

1

36

0.45

0.56

280

0.32

0.53