Figure 2 | Scientific Reports

Figure 2

From: Nucleation and Ostwald Growth of Particles in Fe-O-Al-Ca Melt

Figure 2The alternative text for this image may have been generated using AI.

Particle size distributions in three-dimensional of different samples at 1600 °C after deoxidation for 3900 s. (a) Is for steels with initial Al added amount of 0.05% and (b) is for steels with initial Al added amount of 0.25%.