Figure 7
From: Effect of secondary phase on the electromagnetic shielding effectiveness of magnesium alloy

(0002) macrotextures of the studied alloys: (a) Mg-3Zn 20% rolled and aged for 25 h, (b) Mg-3Sn 20% rolled and aged for 35 h, (c) Mg-5Sn 20% rolled and aged for 35 h, (d)Mg-3Zn 50% rolled and aged for 25 h, (e) Mg-3Sn 50% rolled and aged for 35 h, and (f) Mg-5Sn 20% rolled and aged for 35 h.