Figure 6

(a) Field dependence of magnetostriction measured at 200 K (blue), 270 K (red) and 280 K (black) in a field applied parallel to the Mn2GaC film plane. Panels (b,c,d) combine plots of MS (black circles and left inner scale bar), magnetization (red line and left outer scale bar) and MR (blue squares and right scale bar) measured at (b) 200 K (below T t ), (c,d) 280 K and 270 K (above T t ).