Figure 9

Heat deflection of scPLA or its composites with varying amount of MCH with change in temperature before annealing (a) and after annealing at 160 °C (b).

Heat deflection of scPLA or its composites with varying amount of MCH with change in temperature before annealing (a) and after annealing at 160 °C (b).