Table 2 Theoretical predictions and experimental values of dielectric constants of fluorinated BSTO/PVdF-HFP nanocomposites at a frequency of 1 MHz.
Modified Kerner model | Experimental value | |
|---|---|---|
BaTiO3/PVdF-HFP | 16.9 | 16.7 (±1.1) |
Ba0.8Sr0.2TiO3/PVdF-HFP | 16.9 | 16.5 (±1.4) |
Ba0.6Sr0.4TiO3/PVdF-HFP | 17.5 | 18.4 (±1.7) |
Ba0.4Sr0.6TiO3/PVdF-HFP | 17.0 | 17.2 (±1.9) |
Ba0.2Sr0.8TiO3/PVdF-HFP | 16.7 | 16.6 (±1.8) |
SrTiO3/PVdF-HFP | 17.2 | 16.9 (±2.4) |