Table 2 Relative content of Al sites and their chemical shift obtained from 27Al MAS NMR spectra after deconvolution.

From: Preparation of colourless phosphate glass by stabilising higher Fe[II] in microwave heating

Glass

Chemical shift (ppm)

% of occupancy

Glass

Chemical Shift(ppm)

% of occupancy

GC0Sn

53.32

0.97

GM0Sn

45.79

0.82

14.21

7.03

14.15

4.24

−14.29

91.99

−14.60

94.94

GC0.5Sn

55.23

1.16

GM0.5Sn

53.86

1.16

14.21

9.41

14.30

7.01

−14.40

89.43

−14.63

91.83

GC1Sn

52.56

0.89

GM1Sn

53.98

0.94

15.86

5.59

14.51

4.14

−14.60

93.52

−14.56

94.92

GC1.5Sn

53.59

2.08

GM1.5Sn

56.67

0.28

16.12

6.39

15.22

4.86

−14.51

91.53

−14.44

94.86

GC2Sn

55.46

0.83

   

14.59

4.62

   

−14.94

94.54