Table 1 Structural parameters of SnO2/CX[Y].

From: High capacity and stable all-solid-state Li ion battery using SnO2-embedded nanoporous carbon

Sample

Y (wt%)

Sa (m2/g)

Sa,w (m2/g)

Vp (cm3/g)

Vp,w (cm3/g)

SnO2/C140[Y]

0

61

70

1073

326

279

1073

594

523

2.00

0.56

0.38

2.00

0.78

0.60

SnO2/C45[Y]

0

56

68

72

1093

548

223

220

1093

604

518

489

4.42

1.82

0.92

0.90

4.42

1.94

1.41

1.24

  1. Y: SnO2 content, Sa: Specific surface area, Vp: specific pore volume, Sa,w and Vp,w: calculated values of Sa and Vp under the assumption of a simple mixing of CX and SnO2.